Femtosecond Laser-Induced Formation of Gold-Rich Nanoalloys from the Aqueous Mixture of Gold-Silver Ions
Figure 3
TEM micrograph of samples prepared in this work: Au/Ag = (a) 100/0, (b) 90/10, (c) 75/25, (d) 50/50, (e) 25/75, (f) 10/90, and (g) 0/100. The corresponding particle size distributions were also presented, except for (g) because no particles were found.