Femtosecond Laser-Induced Formation of Gold-Rich Nanoalloys from the Aqueous Mixture of Gold-Silver Ions
Figure 4
High resolution electron micrographs of typical bimetallic AuAg nanoparticles with initial concentration of (a) 25/75, (b) 50/50, and (c) 75/25. Note that fringes pattern confirm the crystalline nature of nanoparticles. (Inset figure: the corresponding FFT images.)