Towards a Reproducible Synthesis of High Aspect Ratio Gold Nanorods
Figure 10
TEM images of gold nanorods prepared with different concentrations of tetrachloroauric acid in the growth solution: 2.5·10−4 M (a), 5·10−4 M (b), 7.5·10−4 M (c), and 1.5·10−3 M (d).