Application of Flow Focusing to the Break-Up of a Magnetite Suspension Jet for the Production of Paramagnetic Microparticles

Table 2

MPs size as a function of polymer and Aerosil concentration (Magnetite 4% w/v, Qt 3 mL/min, Qd 1 mL/h).

FormulationD th ( m) ( m)SD ( m)VC (%)GSD

F24.03.730.5915.961.18
F33.800.3910.341.10
F44.74.940.418.371.09
F54.950.499.861.09
F75.25.550.539.611.10
F86.26.030.6711.061.12
F95.86.090.7512.291.34
F115.85.780.254.391.05