Growth Behaviors of ZnO Nanorods Grown with the Sn-Based Bilayer Catalyst-Covered Substrates
Figure 5
Surface morphologies of ZnO grown at 700°C for 2 h on (a) untreated, (b) 700°C preannealed, and (c) 850°C preannealed Sn/Al substrates by thermal evaporation with a Zn mixture of Zn and ZnO in a weight ratio of 1 : 1. (d) X-ray diffraction patterns of ZnO nanorods grown on three types of Sn/Al substrates.