Research Article

ZnO Nanowire Formation by Two-Step Deposition Method Using Energy-Controlled Hollow-Type Magnetron RF Plasma

Figure 4

SEM images with deposition time as a parameter in case of = 60 s: = (a) 0 s, (b) 60 s, (c) 300 s, and (d) 600 s.
850930.fig.004a
(a)
850930.fig.004b
(b)
850930.fig.004c
(c)
850930.fig.004d
(d)