Fabrication of Biodegradable Polyester Nanocomposites by Electrospinning for Tissue Engineering
Figure 12
pH changes of PLLA, PLLA/NHAP (80 : 20, w/w) and PLLA/MNHAP (80 : 20, w/w) scaffold during in vitro degradation. Reproduced from Medical Engineering & Physics with permission from Elsevier [56].