Table 3:
Micro-calorimeter results showing decomposition temperature (
o
C) and heat release rate (W/g).
Material
Decomposition temperature (
°
C)
HRR (W/g)
PE
502.7
1323.2
PE/15 mg AlN
511.8
1067.4
PE/30 mg AlN
501.8
998.7
PE/45 mg AlN
505.6
972.6