A Decrease in NiO-MgO Phase Through Its Solid Solution Equilibrium with Tetragonal : Effect on Catalytic Partial Oxidation of Methane
Figure 9
XRD patterns of the three used catalysts after POM for 50 h at 850°C (with reference to Figure 7): Tthe tetragonal phase, •La-Sr-O, ∆SrCO3, ♦NiO/MgO solution, ◊Ni0, and Ccarbon.