Review Article

Matrix-Assisted Pulsed Laser Thin Film Deposition by Using Nd:YAG Laser

Figure 6

POOPT thin film deposited on a glass slide with MAPLE technique with the following layout/deposition parameters: target: POOPT 0.56 wt.% in chloroform; target temperature: −187°C; pressure: 2.3 10−7 Torr; laser wavelength: 532 nm; pulse repetition rate: 10 pulse/s; pulse duration: 6 ns; pulse energy: 68 mJ; beam spot size: 0.5 cm2; total pulses: 20000; scanned target area: 2 cm2.
395436.fig.006