Research Article

Effect of Titanium Substitution on Magnetic Properties and Microstructure of Nanocrystalline Monophase Nd-Fe-B Magnets

Figure 4

TEM images of Nd12.3Fe80.7Ti1B6 (a) and Nd12.3Fe81.7B6 (b) ribbons annealed at 600°C for 10 min.
425028.fig.004a
(a)
425028.fig.004b
(b)