Review Article

Synthesis, Characterization, and Applications of ZnO Nanowires

Figure 9

Raman spectra of the ZnO structures obtained by the hydrothermal method at 130°C for (a) 30 min, (b) 60 min, (c) 120 min, and (d) 180 min (reproduced with permission from [125] © 2010 Elsevier).
624520.fig.009