Research Article

Biocompatibility of Nanoporous TiO2 Coating on NiTi Alloy Prepared via Dealloying Method

Figure 1

SEM images of the surface morphologies of NiTi alloy dealloyed for 0 h, 4 h, 6 h, 9 h, and 15 h.
731592.fig.001a
(a)
731592.fig.001b
(b)
731592.fig.001c
(c)
731592.fig.001d
(d)
731592.fig.001e
(e)