Research Article
Measuring of Electrical Properties of MWNT-Reinforced PAN Nanocomposites
Table 1
Parameters of electrospinning process.
| | 10% PAN | 10% PAN 0.2% CNT | 10% PAN 0.4% CNT | 10% PAN 0.5% CNT | 10% PAN 0.7% CNT | 10% PAN 1.0% CNT | 10% PAN 1.5% CNT |
| Voltage (kV) | 11 | 12 | 12.5 | 11 | 14 | 14 | 12 | Gap needle collector (cm) | 30 | 30 | 30 | 30 | 30 | 30 | 30 | Feed rate (mL/h) | 0.354 | 0.212 | 0.212 | 0.283 | 0.424 | 0.424 | 0.283 | Period of spinning (min) | 60 | 60 | 60 | 60 | 60 | 60 | 60 |
|
|