Weight loss and amount of carbon.
| Sample | Weight loss (% w/w) | Weight loss (% w/w) | Residue (% w/w) | Carbon | 25–150°C | 150–600 | 600°C | % | mmol·g-1 |
| SBA-16 | 13.1 | — | 85 | | 0.21 | M-PTES | 3.4 | 2.8 | 93 | | 1.76 | T-PTES | 1.3 | 7.2 | 91 | | 6.57 |
|
|