Research Article

On the Origin of Light Emission in Silicon Rich Oxide Obtained by Low-Pressure Chemical Vapor Deposition

Figure 12

Cathode-luminescence for SRO10, 20, and 30 after annealing at 1,100°C for 180 minutes.
890701.fig.0012