Research Article

On the Origin of Light Emission in Silicon Rich Oxide Obtained by Low-Pressure Chemical Vapor Deposition

Figure 8

Excitation wavelength with the detector centered at 750 nm for SRO10, 20, and 30 annealed at 1,100°C for 180 minutes.
890701.fig.008