Control of FeAl Composition Produced by SPS Reactive Sintering from Mechanically Activated Powder Mixture

Figure 9

SEM (BSE mode) micrographs of a homogeneous single phase FeAl after thermal treatment (1000°C, 30 min) on sample containing Fe + Fe2Al5 + FeAl phases presented in Figures 6(e) and 7(c).