The Investigation of Bioactivity and Mechanical Properties of Glass Ionomer Cements Prepared from Al2O3-SiO2 Glass and Poly(γ-glutamic acid)
Figure 4
SEM micrographs and EDX spectra of the SBF-unsoaked cement surface, the deposits precipitating on the surfaces of cements, after soaking in SBF for 7 days. PGA concentration of the SBF-unsoaked cement is 10% m/m.