Research Article

Cytocompatibility of Plasma and Thermally Treated Biopolymers

Figure 7

Dependence of the number of adhered and proliferated cells after 1, 2, 5, and 7 days from seeding on pristine PLLA and PMP and PLLA and PMP treated in plasma (power 5 and 10 W, time 40 and 240 s). The values for tissue polystyrene as standard material (TCPS) were also introduced for comparison.
238742.fig.007