Research Article
Preparation, Characterization, and Properties of In Situ Formed Graphene Oxide/Phenol Formaldehyde Nanocomposites
Table 1
Results of TGA curves of PF and GO/PF in situ nanocomposites.
| ||||||||||||||||||||||||||||||||||||||||