Research Article

Processing of CNTs Reinforced Al-Based Nanocomposites Using Different Consolidation Techniques

Figure 3

Shows densification (a) and hardness (b) of as-received Al-7Si-0.3Mg alloy sintered at 400, 450, and 500°C using microwave, HIP, and SPS techniques.
370785.fig.003a
(a)
370785.fig.003b
(b)