Processing of CNTs Reinforced Al-Based Nanocomposites Using Different Consolidation Techniques
Figure 6
Shows densification (a) and hardness (b) of Al-12Si-0.3Mg + 0.5 wt% CNT powder milled for 5 h and sintered at 400, 450, and 500°C using microwave, HIP, and SPS techniques.