Processing of CNTs Reinforced Al-Based Nanocomposites Using Different Consolidation Techniques
Figure 7
SEM micrographs of as-received Al-7Si-0.3Mg (alloy 1) sintered at 500°C using (a) microwave (μW), (b) hot isostatic pressing (HIP), and (c) Spark plasma (SPS).