Research Article

A Convenient and Templated Method for the Fabrication of Monodisperse Micrometer Hollow Titania Spheres

Figure 2

TG curves of the as-synthesized PSA/TiO2 composite spheres under different TBOT volumes: (a) 0.5 g; (b) 1.0 g; (c) 1.5 g, and (d) 2.0 g. The composite spheres were heated from the ambient temperature to 800°C at a rate of 5°C/min under oxygen purge.
372058.fig.002