Research Article

Surface Modification on the Sputtering-Deposited ZnO Layer for ZnO-Based Schottky Diode

Figure 10

RTPL spectra of the (a) untreated, (b) H2O2-treated, and (c) (NH4)2Sx-treated ZnO layers.
560542.fig.0010a
(a)
560542.fig.0010b
(b)
560542.fig.0010c
(c)