Research Article

Surface Modification on the Sputtering-Deposited ZnO Layer for ZnO-Based Schottky Diode

Figure 3

I-V characteristics of the ZnO layer contact to the Ni/Au metal with and without an additive preetching process prior to the surface treatment using the dilute HCl solution (the inset figure highlights the current in logarithmic scale).
560542.fig.003