Research Article

Electrospun Hyaluronan-Gelatin Nanofibrous Matrix for Nerve Tissue Engineering

Figure 5

Quantification of RT4-D6P2T Schwann cells on Gel and HA-Gel matrices. The MTT assay was used to quantify cell attachment and proliferation on Gel and HA-Gel. (a) The attachment of RT4-D6P2T Schwann cells on various matrices after culturing for up to 4 hrs. (b) The viability of RT4-D6P2T Schwann cells on various matrices after culturing for up to 6 days. The data are presented as the means ± SD, . No statistically significant differences in cell attachment or proliferation on the HA-Gel and Gel were found.
613638.fig.005a
(a)
613638.fig.005b
(b)