Research Article

Reactive Spark Plasma Sintering: Successes and Challenges of Nanomaterial Synthesis

Figure 12

Microstructure of the B4C-TiB2 composites SPS-ed using different electric current values ((a)—1100 A, (b)—1150 A, and (c)—1200 A) (reprinted from [49], Copyright (2012), with permission from Elsevier).
625218.fig.0012a
(a)
625218.fig.0012b
(b)
625218.fig.0012c
(c)