Research Article
Effects of Chitosan Alkali Pretreatment on the Preparation of Electrospun PCL/Chitosan Blend Nanofibrous Scaffolds for Tissue Engineering Application
Table 1
Electrospinning of PCL/chitosan blend and effect on required voltage.
| PCL/chitosan blend | Applied voltage |
| 8% PCL and 2.5% untreated chitosan (70/30) | 21 | 8% PCL and 7% treated chitosan (70/30) | 25 | 8% PCL and 2.5% untreated chitosan (50/50) | — | 8% PCL and 7% treated chitosan (50/50) | 28 |
|
|