Research Article
Triple-Component Drug-Loaded Nanocomposites Prepared Using a Modified Coaxial Electrospinning
Table 1
Parameters of the electrospinning processes and their products.
| No. | Electrospinning | PVP content (%) | Flow rate (mL/h) | Morphologyb | Diameter (nm) | Sheath fluida | Core fluid | Ratio |
| F1 | Single | 10.5 | 0.0 | 1.0 | 0 | Linear/thick fibers | |
| F2 | Coaxial | 10.5 | 0.1 | 0.9 | 0.11 | Linear | | F3 | Coaxial | 10.5 | 0.2 | 0.8 | 0.25 | Beads-on-a-string | | F4 | Coaxial | 0 | 0.1 | 0.9 | 0.11 | Linear | | F5 | Coaxial | 22.7 | 0.1 | 0.9 | 0.11 | Linear | |
|
|
Sheath fluid was DMAc.
bIn this column, ‘‘linear’’ morphology refers to nanofibers with few beads or spindles on them.
|