Research Article

Effect of Mechanical Deformation on Thermoelectric Properties of p-Type Alloys

Figure 8

Change of the power factor of (Bi0.225Sb0.775)2Te3 alloys of as-quenched ingot and the 10 times cold-pressing with annealing time at 573 K.
868540.fig.008