Research Article

Magnetic Properties and Microstructure of FeOx/Fe/FePt and FeOx/FePt Films

Figure 4

In-plane and out-of-plane magnetic hysteresis loops of FeOx(P)/Fe/FePt trilayer further annealed at 500°C with = (a) 1%, (b) 3%, and (c) 7% and 800°C with = (d) 1%, (e) 3%, and (f) 7%.