Research Article

Dielectric Properties and Characterisation of Titanium Dioxide Obtained by Different Chemistry Methods

Figure 8

The frequency dependence of dielectric constant (a) and loss tangent (b) measured at 20°C for investigated rutile samples annealed for 2 h at 850°C (synthesis ) and at 900°C (syntheses and (3)).
124814.fig.008a
(a)
124814.fig.008b
(b)