Research Article

Characterization of the Nanoporous Template Using Anodic Alumina Method

Figure 10

Optical transmittance of AAO/ITO/glass structure at bias voltages of 20 V, 40 V, 60 V, 80 V, 100 V, and 120 V after posttreatment annealing.
130716.fig.0010