Room Temperature Optical Constants and Band Gap Evolution of Phase Pure M1-VO2 Thin Films Deposited at Different Oxygen Partial Pressures by Reactive Magnetron Sputtering
Figure 1
Raman (a) and XRD (b) spectra for VO2 films deposited at different O2-Ar ratios.