Research Article

Size, Temperature, and Strain-Rate Dependence on Tensile Mechanical Behaviors of Ni3Sn4 Intermetallic Compound Using Molecular Dynamics Simulation

Figure 7

Stress-strain responses of the three Ni3Sn4 nanowire models of three different sizes at 300 K, 500 K, and 700 K and the strain rate of 10−4% ps−1.
214510.fig.007a
(a) -axis
214510.fig.007b
(b) -axis
214510.fig.007c
(c) -axis