Research Article

Nanopolycrystalline Diamond Sintered from Onion-Like Carbon

Figure 7

Properties of nPCD sintered from OLCs annealed at 900–1400°C: (a) Vickers hardness; (b) density; (c) grain size.
271494.fig.007a
(a)
271494.fig.007b
(b)
271494.fig.007c
(c)