Investigation of the Microstructural and Thermoelectric Properties of the Composition for Thermoelectric Power Generation Applications

Figure 2

Powder XRD of (GeTe)0.95(Bi2Te3)0.05 following hand crushing for maximal powder particles size of 50 and 250 μm and following 10 and 20-cycle ball milling of 10 minutes at 700 RPM/10 min.