Research Article

Investigation of the Microstructural and Thermoelectric Properties of the Composition for Thermoelectric Power Generation Applications

Figure 6

Temperature dependence of the lattice thermal conductivity, , for (GeTe)0.95(Bi2Te3)0.05 following hand crushing for maximal powder particles size of 50 and 250 μm and hot pressing at 650°C (50 μm/650°C and 250 μm/650°C, resp.) and for 250 μm hot pressed powder at 450°C (250 μm/450°C).