Optimization of the Electrodeposition Parameters to Improve the Stoichiometry of Films for Solar Applications Using the Taguchi Method

Table 4

Sulfur to indium (S/In) molar ratios from EDS.

UniformityL27 orthogonal array experimentS/In molar ratio

11.1556
21.2567
31.2313
41.3697
51.3132
61.3196
71.6671
81.4445
91.4097
101.2559
111.3510
121.3297
131.3818
141.3910
151.4462
161.3684
171.4012
181.46
191.2894
201.2354
211.4032
221.3520
231.2807
241.4150
251.4108
261.2442
271.4221

  Uniform In2S3 films.
  Nonuniform In2S3 films.