Research Article
Synthesis and Optical Properties of Thiol Functionalized CdSe/ZnS (Core/Shell) Quantum Dots by Ligand Exchange
Table 1
The optical properties of as-synthesized CdSe QDs with growth at 250°C.
| Growth time of samples | Emission peak area | Full width half maximum (FWHM) | OD
| Quantum yield (QY) |
| 10 min | 83710 | 30.0 | 0.120 | 0.69 | 30 min | 180819 | 35.1 | 0.126 | 1.46 | 60 min | 248743 | 40.8 | 0.125 | 2.00 | 90 min | 250027 | 42.7 | 0.120 | 2.07 | 120 min | 387545 | 43.3 | 0.119 | 3.30 |
|
|