Structural and Electrical Properties of the YSZ/STO/YSZ Heterostructure

Figure 3

Impedance spectra (open symbols) and corresponding fit curves (lines) measured at 500°C, 550°C, and 600°C for the YSZ/STO/YSZ epitaxial films on MgO substrates in dry air; the inset shows an equivalent circuit.