Research Article

Fabrication of Core-Shell Structural SiO2@H3[PM12O40] Material and Its Catalytic Activity

Figure 7

Degradation of ST under different catalyst ((a) SiO2@PW12, (b) SiO2@PMo12).
835931.fig.007a
(a)
835931.fig.007b
(b)