Preparation and Characterization of Au/Pd Modified-TiO2 Photocatalysts for Phenol and Toluene Degradation under Visible Light—The Effect of Calcination Temperature

Figure 3

XRD pattern in ranges (a) 20–80° and (b) 37–46° of sample 0.5 Pd/1.25 Au-TiO2 calcinated from 350 to 700°C.