Research Article

Preparation and Microstructure Analysis of TiC-Derived Carbons with Hierarchical Pore Structure

Figure 1

(a) XRD patterns of TiC and (b) CDC samples synthesized at various temperatures. Complete conversion of TiC to carbon takes place at 600°C and above. Broad peaks show the highly amorphous nature of the carbon produced from TiC.