AFM images (10 × 10 μm2) of the surface roughness of etched glass. (a) shows glass surface before etching; (b) shows glass etched at 50 W for 5 min; (c) shows glass etched at 100 W for 5 min; (d) shows glass etched at 200 W for 5 min.