DMA and Conductivity Studies in PVA:NH4SCN:DMSO:MWNT Nanocomposite Polymer Dried Gel Electrolytes
Table 1
Peak values of loss modulus at 5 Hz for different concentration of MWNT filled PVA:NH4SCN nanocomposite polymer electrolytes.
| Samples composition | Transition temperatures | | | | | |
| PVA:NH4SCN polymer gel electrolyte | 102 | 119.1 | 136 | 143 | 162 |
| PVA:NH4SCN:2 wt% MWNT filled composite gel electrolyte | 98.8 | 123.6 | 137.1 | 147 | 160 |
| PVA:NH4SCN:4 wt% MWNT filled composite gel electrolyte | 96.3 | 122 | 138 | 150 | 163 |
| PVA:NH4SCN:6 wt% MWNT filled composite gel electrolyte | 87.6 | 119.2 | ⋯ | 144 | 159 |
| PVA:NH4SCN:8 wt% MWNT filled composite gel electrolyte | 103.6 | 122.2 | 136 | 148 | 162 |
|
|