Research Article

Subzero Temperature Dip-Coating of Sol-Gel Vanadium Pentoxide: Effect of the Deposition Temperature on the Film Structure, Morphology, and Electrochromic Properties

Figure 2

XRD pattern of the vanadium oxide films, dip-coated at −10°C and annealed at 300°C (a) and 500°C (b). X-ray diffraction signal of an orthorhombic V2O5 film (ICDD 41-1426) on an ITO covered glass substrate, annealed at 500°C for one hour. The signal from the glass substrate has been subtracted. The fit (red line) includes the contributions from V2O5 and ITO to the signal.
(a)
(b)