Preparation of Lanthanum Oxide and Lanthanum Oxycarbonate Layers on Titanium by Electrodeposition with Organic Solution

Figure 16

Yields of 30 min depositions with 0.092 mg/mL of La3+ ions at 200, 400, 600, and 1000 V.